Rob Davey Posted July 12, 2006 Share Posted July 12, 2006 Ok im spraying a splitter. I've filled in a couple of marks with P** filler (can't remember the number) smoothed it down and put primer on it. All was fine and i left it two days to dry. Now after putting on the paint the marks are showing through a little as if the filler has shrunk? WTF? It was fine before the main paint - any ideas why this has happened? Quote Link to comment Share on other sites More sharing options...
Supe Posted July 12, 2006 Share Posted July 12, 2006 mm, think you need to sand it down again and then wet and dry it workin the grits of the sandpaper up until it is completely smooth. Quote Link to comment Share on other sites More sharing options...